tow bar
by G Walker - 24/08/26 06:52 PM
|
|
|
|
|
Forums39
Topics49,836
Posts837,251
Members9,596
| |
Most Online1,063 Jun 14th, 2026
|
|
If a specific post was interesting or useful to you, we recommend that you Like that post. It tells the post author, and others, that you found the information valuable. Clicking Like is another way to let others know that you enjoy it without leaving a comment.
Log in to join the conversation and Like this content.
|
|
|
|
+8Rich (Aug 3rd 2026) |
|
Total Likes: 1 |
|
Re: Exhaust flexible rubber test
#847544
Aug 3rd a 01:41 PM
|
| by Herrie |
| Herrie |
Hi RichardV6
I am afraid that's not a good idea.
Stainless steel and aluminium hate each others present. Stainless eats the Aluminium fast. Cause : Electrolyse. Especially at this point where you have very often water.
A former owner of my M3W used SS refits to connect the body to the frame. All aluminium is damaged around the refits. You can see the paint 'bubbling'.
So always use the galvanised bobbins and not the SS ones. Zinc - Galvanise material - is nearer to aluminium in the periodic table. Even Tefgel will not help here connecting surface is too big.
|
|
|
|
|
|