Stainless doesn't mean rust free. stainless is particularly sensitive to chloride pin hole corrosion. Had no idea stainless rusted , I thought if you get high quality 304 grade stainless it didn't rust . 
Last edited by madmax; 02/03/20 07:14 PM.
Geneva 2016 plus 8' The Green Godess' 4 side exits .
|
|
|
|
|
Joined: Nov 2011
Posts: 7,342 Likes: 49
Talk Morgan Guru
|
Talk Morgan Guru
Joined: Nov 2011
Posts: 7,342 Likes: 49 |
Stainless doesn't mean rust free. stainless is particularly sensitive to chloride pin hole corrosion. Better check the Delorean..... 
A Morgan Identified Fastidious Owner... 2011 4/4 Bespoke, 1981 Delorean, Auburn Boat Tail
|
|
|
|
|
Joined: Aug 2014
Posts: 5,587
Charter Member
|
Charter Member
Joined: Aug 2014
Posts: 5,587 |
Stainless doesn't mean rust free. stainless is particularly sensitive to chloride pin hole corrosion. Better check the Delorean.....  
Geneva 2016 plus 8' The Green Godess' 4 side exits .
|
|
|
|
|
Joined: Nov 2015
Posts: 8,672 Likes: 489
Just barreling along Needs to Get Out More!
|
Just barreling along Needs to Get Out More!
Joined: Nov 2015
Posts: 8,672 Likes: 489 |
Stainless doesn't mean rust free. stainless is particularly sensitive to chloride pin hole corrosion. Had no idea stainless rusted , I thought if you get high quality 304 grade stainless it didn't rust .  Beware, 304 is cooking grade stuff used for wall ties & the like in construction - go for 316 if you can get it
Jon M
|
|
|
|
|
Joined: May 2017
Posts: 1,633 Likes: 62
Talk Morgan Enthusiast
|
Talk Morgan Enthusiast
Joined: May 2017
Posts: 1,633 Likes: 62 |
Jon is absolutely right , here in construction within .7 of a kilometre of the sea you must only use 316, and in marine it is normal for all fastenings, though many components are now using duplex 2205 .
99 plus 8 indigo
|
|
|
|
|
Joined: Jul 2007
Posts: 27,810 Likes: 749
Member of the Inner Circle
|
Member of the Inner Circle
Joined: Jul 2007
Posts: 27,810 Likes: 749 |
Or 316L but of course it is more brittle than 304. If you have the cash how about Titanium stabilised palladium. I once sold an oyster farm a plate heat exchange pasteuriser for sea water in TiPd.
JohnV6 2022 CX Plus Four 2025 Renault Scenic Alpine etech "Yvette"
|
|
|
|
|