With all the crap going on in life and the world, progress has pretty much halted....Until today, when I picked up my splined shafts for the transfer case and intermediate shaft. They are now Carbonitrided and the splines are hardened to about 58rc and the rest is between 43-45rc. The steel started at around 18rc.

I can now complete the assembly of the transfer case and the bearing housing of the intermediate shaft.